Kas ir Galvanic Corrosion?

Galvanic corrosion occurs when dissimilar metals contact in electrolyte; more active metal (anode) corrodes preferentially.

Soli pa solim ceļvedis

  1. 1Input two metals and galvanic series position
  2. 2Calculate galvanic potential
  3. 3Determine which metal corrodes and rate

Worked Examples

Ievade
Zinc (anode) + steel (cathode) in seawater
Rezultāts
Zinc sacrificially corrodes, protecting steel (intentional use)

Common Mistakes to Avoid

  • Assuming only one metal corrodes (wrong)
  • Not understanding sacrificial anode concept

Frequently Asked Questions

How do you prevent galvanic corrosion?

Use same metal, isolate with non-conductive gasket, or apply protective coating.